Surface Area | 100-200 M2/g |
---|---|
Active Component | Palladium (Pd) |
Pore Volume | 0.3-0.5 Cm3/g |
Application | Selective Hydrogenation Of C8/C9 Hydrocarbons |
Particle Size | 1-3 Mm |
Support Material | Alumina Or Silica-alumina |
---|---|
Catalyst Lifespan | ≥ 3 Years |
Pore Diameter | 30-80 Å |
Pore Volume | ≥ 0.35 ML/g |
Active Component | Pd, Pt, Ni, Or Co |
Support Material | Aluminum Oxide (Al2O3) |
---|---|
Stability | Excellent Stability Under Harsh Conditions |
Surface Area | High Surface Area For Efficient Catalytic Activity |
Catalyst Type | Supported Metal Catalyst |
Particle Size | Narrow Particle Size Distribution |
Active Component Loading | ≥ 2 Wt% |
---|---|
Active Component | Pd, Pt, Ni, Or Co |
Hydrogenation Selectivity | ≥ 95% |
Support Material Content | ≥ 90 Wt% |
Operating Temperature | 150-250°C |
Appearance | Gray Or Black Cylindrical Particles |
---|---|
Operating Temperature | 150-250°C |
Hydrogenation Selectivity | ≥ 95% |
Catalyst Lifespan | ≥ 3 Years |
Active Component Loading | ≥ 2 Wt% |
Particle Size | 1-3 Mm |
---|---|
Appearance | Dark Gray To Black Solid |
Surface Area | 100-200 M2/g |
Active Component | Palladium (Pd) |
Application | Selective Hydrogenation Of C8/C9 Hydrocarbons |
Catalyst Lifespan | ≥ 3 Years |
---|---|
Appearance | Gray Or Black Cylindrical Particles |
Operating Pressure | 1-10 MPa |
Particle Size | 1.5-3.0 Mm |
Active Component | Pd, Pt, Ni, Or Co |
Shape | Spherical |
---|---|
Support Material | Aluminum Oxide (Al2O3) |
Activity | High Activity For C3 Hydrogenation |
Surface Area | High Surface Area For Efficient Catalytic Activity |
Selectivity | High Selectivity C3 Hydrogenation |
Support Material | Aluminum Oxide (Al2O3) |
---|---|
Selectivity | High Selectivity C3 Hydrogenation |
Catalyst Type | Supported Metal Catalyst |
Stability | Excellent Stability Under Harsh Conditions |
Activity | High Activity For C3 Hydrogenation |
Support Material | Alumina Or Silica-alumina |
---|---|
Pore Volume | ≥ 0.35 ML/g |
Bulk Density | 0.65-0.75 G/cm3 |
Support Material Content | ≥ 90 Wt% |
Hydrogenation Selectivity | ≥ 95% |