Keywords [ solid catalyst ] match 308 products.
Active Component Content C4/C5 Hydrogenation Catalysts In Gray Or Black Cylindrical Particles

Active Component Content C4/C5 Hydrogenation Catalysts In Gray Or Black Cylindrical Particles

Support Material Alumina Or Silica-alumina
Catalyst Lifespan ≥ 3 Years
Pore Diameter 30-80 Å
Pore Volume ≥ 0.35 ML/g
Active Component Pd, Pt, Ni, Or Co
High Pressure Precious Metal Hydrogenation Catalyst / 1-10 MPa h2 catalyst

High Pressure Precious Metal Hydrogenation Catalyst / 1-10 MPa h2 catalyst

Bulk Density 0.65-0.75 G/cm3
Support Material Alumina Or Silica-alumina
Active Component Pd, Pt, Ni, Or Co
Catalyst Lifespan ≥ 3 Years
Particle Size 1.5-3.0 Mm
Pd/Pt/Ni/Co Hydrogenation Catalyst Gray / Black Particles 150-250°C Operating Temperature

Pd/Pt/Ni/Co Hydrogenation Catalyst Gray / Black Particles 150-250°C Operating Temperature

Catalyst Lifespan ≥ 3 Years
Active Component Pd, Pt, Ni, Or Co
Particle Size 1.5-3.0 Mm
Hydrogenation Selectivity ≥ 95%
Pore Volume ≥ 0.35 ML/g
0.55G/cm3 2-Ethylanthraquinone Hydrogenation Catalyst Insoluble In Water Shelf Life 2 Years Density 0.55

0.55G/cm3 2-Ethylanthraquinone Hydrogenation Catalyst Insoluble In Water Shelf Life 2 Years Density 0.55

Density 0.55 G/cm3
Shelf Life 2 Years
Storage Store In Dry Place
Application Catalyst For 2-ethylanthraquinone Hydrogenation Reactions
Solubility Insoluble In Water
Alumina Supported C4/C5 Nickel Hydrogenation Catalyst ≥ 0.35 ML/G Pore Volume

Alumina Supported C4/C5 Nickel Hydrogenation Catalyst ≥ 0.35 ML/G Pore Volume

Support Material Alumina Or Silica-alumina
Pore Volume ≥ 0.35 ML/g
Bulk Density 0.65-0.75 G/cm3
Support Material Content ≥ 90 Wt%
Hydrogenation Selectivity ≥ 95%
Reaction Selectivity Cracked Gasoline Hydrogenation Catalyst Spherical Shape 150M2/g-200M2/g

Reaction Selectivity Cracked Gasoline Hydrogenation Catalyst Spherical Shape 150M2/g-200M2/g

Pore Size 0.3-0.5 Nm
Surface Area 150-200 M2/g
Composition Nickel, Cobalt, Molybdenum, Alumina
Bulk Density 0.7-0.9 G/cm3
Reaction Selectivity 95-98%
Spherical Surface Area Hydrogenation Catalyst H2 For Cracked Gasoline Processing

Spherical Surface Area Hydrogenation Catalyst H2 For Cracked Gasoline Processing

Catalyst Life 2-3 Years
Reaction Selectivity 95-98%
Application Hydrogenation Of Cracked Gasoline
Pore Size 0.3-0.5 Nm
Bulk Density 0.7-0.9 G/cm3
Surface Area 150-200 M2/g Cracked Gasoline Hydrogenation Catalyst with 95-98% Reaction Selectivity

Surface Area 150-200 M2/g Cracked Gasoline Hydrogenation Catalyst with 95-98% Reaction Selectivity

Catalyst Life 2-3 Years
Pore Size 0.3-0.5 Nm
Reaction Selectivity 95-98%
Application Hydrogenation Of Cracked Gasoline
Size 1-3 Mm
98% Purity Hydrogenation Catalyst for Enhanced Beverage and Food Production

98% Purity Hydrogenation Catalyst for Enhanced Beverage and Food Production

Density 0.55 G/cm3
Solubility Insoluble In Water
Purity ≥ 98%
Application Catalyst For 2-ethylanthraquinone Hydrogenation Reactions
Storage Store In Dry Place
Surface Area Hydrogenation Catalyst 0.3-0.5 Nm for Enhanced Selectivity

Surface Area Hydrogenation Catalyst 0.3-0.5 Nm for Enhanced Selectivity

Shape Spherical
Pore Size 0.3-0.5 Nm
Composition Nickel, Cobalt, Molybdenum, Alumina
Reaction Selectivity 95-98%
Size 1-3 Mm