| Surface Area | 100-200 M2/g |
|---|---|
| Particle Size | 1-3 Mm |
| Active Component | Palladium (Pd) |
| Application | Selective Hydrogenation Of C8/C9 Hydrocarbons |
| Promoter | Aluminum Oxide (Al2O3) |
| Application | Selective Hydrogenation Of C8/C9 Hydrocarbons |
|---|---|
| Particle Size | 1-3 Mm |
| Appearance | Dark Gray To Black Solid |
| Promoter | Aluminum Oxide (Al2O3) |
| Active Component | Palladium (Pd) |
| Application | Selective Hydrogenation Of C8/C9 Hydrocarbons |
|---|---|
| Surface Area | 100-200 M2/g |
| Appearance | Dark Gray To Black Solid |
| Active Component | Palladium (Pd) |
| Particle Size | 1-3 Mm |
| Catalyst Lifespan | ≥ 3 Years |
|---|---|
| Appearance | Gray Or Black Cylindrical Particles |
| Operating Pressure | 1-10 MPa |
| Particle Size | 1.5-3.0 Mm |
| Active Component | Pd, Pt, Ni, Or Co |
| Particle Size | 1-3 Mm |
|---|---|
| Application | Selective Hydrogenation Of C8/C9 Hydrocarbons |
| Promoter | Aluminum Oxide (Al2O3) |
| Surface Area | 100-200 M2/g |
| Active Component | Palladium (Pd) |
| Operating Pressure | 1-10 MPa |
|---|---|
| Pore Volume | ≥ 0.35 ML/g |
| Pore Diameter | 30-80 Å |
| Appearance | Gray Or Black Cylindrical Particles |
| Particle Size | 1.5-3.0 Mm |
| Operating Pressure | 1-10 MPa |
|---|---|
| Surface Area | ≥ 150 M2/g |
| Active Component Loading | ≥ 2 Wt% |
| Pore Volume | ≥ 0.35 ML/g |
| Support Material Content | ≥ 90 Wt% |
| Active Component | Pd, Pt, Ni, Or Co |
|---|---|
| Particle Size | 1.5-3.0 Mm |
| Support Material | Alumina Or Silica-alumina |
| Active Component Loading | ≥ 2 Wt% |
| Operating Temperature | 150-250°C |